Prieto-Torres, OmairaOmairaPrieto-TorresCarvajal-Garzón, CristhianCristhianCarvajal-GarzónPulido, CamiloCamiloPulidoDávila-Sánchez, AndrésAndrésDávila-SánchezGonzalez-Vaca, ClaudiaClaudiaGonzalez-VacaArrais, Cesar Augusto GalvãoCesar Augusto GalvãoArrais2026-10-182026-10-182026-01-1110.1111/jopr.70085https://repositorio.unicoc.edu.co/handle/SII-Unicoc/321441521400To evaluate the effect of different self-etching primer (Monobond Etch & Prime-MEP) application protocols and aging on micro shear bond strength (µSBS) and surface etching patterns of zirconia-reinforced lithium silicate (ZLS) and lithium disilicate (LD) ceramics.To evaluate the effect of different self-etching primer (Monobond Etch & Prime-MEP) application protocols and aging on micro shear bond strength (µSBS) and surface etching patterns of zirconia-reinforced lithium silicate (ZLS) and lithium disilicate (LD) ceramics.9 ppapplication/pdfenCAD‐CAM ceramicself‐etching primershear bond strengthsurface treatmentzirconia‐reinforced lithium‐silicateEstudios primariosProlonged application methods of self-etching primer: Effect of aging on micro-shear bond strength to lithium disilicate and zirconia-reinforced lithium silicate ceramics.Métodos prolongados de aplicación de imprimación autograbante: Efecto del envejecimiento en la resistencia al microcorte de unión a cerámicas de disilicato de litio y silicato de litio reforzado con zirconia.journal articleCAD‐CAM ceramicself‐etching primershear bond strengthsurface treatmentzirconia‐reinforced l...restrictedAccess